Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 30 sec | 30 sec | ASTM D495 |
Plenco 50130 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat.. |
|||
Arc Resistance | 30 sec | 30 sec | ASTM D495 |
Plenco 51240 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P.. |
|||
Arc Resistance | 30 sec | 30 sec | ASTM D495 |
Plenco 51335 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51335 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in black only.Information .. |
|||
Arc Resistance | 30 - 80 sec | 30 - 80 sec | ASTM D495 |
Covestro Makrolon® 8325 Polycarbonate High viscosity injection molding and extrusion grade with 20% standard glass fibers and easy mold release, high strength and stiffness.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |