Polymer Property : Arc Resistance = 57 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 57 sec
57 sec
ASTM D495
Plenco 3554 Phenolic, Granular, Compression Molded
PLENCO 03554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 03554 is available in black. It is UL listed. 03554 is a re-numbe..