Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 3554 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 3554 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 03554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 03554 is available in black. It is UL listed. 03554 is a re-number of 06554 formulation.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.580 g/cc
0.0210 lb/in³
ASTM D1895
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Water Absorption 0.45 %
0.45 %
ASTM D570
Linear Mold Shrinkage 0.0044 cm/cm
0.0044 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 75
75
ASTM D785
Tensile Strength, Ultimate 56.0 MPa
8120 psi
ASTM D638
Elongation at Break 0.89 %
0.89 %
ASTM D638
Tensile Modulus 8.30 GPa
1200 ksi
ASTM D638
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 7.70 GPa
1120 ksi
ASTM D790
Compressive Strength 155 MPa
22500 psi
ASTM D695
Izod Impact, Notched 0.226 J/cm
0.423 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.224 J/cm²
1.07 ft-lb/in²
ASTM D256
Impact 150
150
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 99.0 µm/m-°C

@Temperature 40.0 - 130 °C
55.0 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.370 W/m-K

@Temperature 100 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 190 °C
374 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 25 %
25 %
ASTM D2863
Shrinkage 0.143 %
0.143 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.10e+12 ohm-cm
2.10e+12 ohm-cm
ASTM D247
Dielectric Constant 4.5
4.5
ASTM D150
Dielectric Strength 16.2 kV/mm
411 kV/in
Short Time; ASTM D149
Dissipation Factor 0.040
0.040
ASTM D150
Arc Resistance 57 sec
57 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved