Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 25 sec | 25 sec | ASTM D495 |
Plenco 5482 Phenolic, Granular, Injection Molded PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect.. |
|||
Arc Resistance | 25 sec | 25 sec | Absolute Drying; ASTM-D495 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 25 sec | 25 sec | Absolute Drying; ASTM-D495 |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 25 sec | 25 sec | ASTM-D495 |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |