Polymer Property : Arc Resistance = 160 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 26.0 - 160 sec
26.0 - 160 sec
Average value: 110 sec Grade Count:7
Overview of materials for Phenolic, Novolac, Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o..
Arc Resistance 112 - 160 sec
112 - 160 sec
Average value: 131 sec Grade Count:5
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..