Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 26.0 - 160 sec | 26.0 - 160 sec | Average value: 110 sec Grade Count:7 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Arc Resistance | 112 - 160 sec | 112 - 160 sec | Average value: 131 sec Grade Count:5 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |