Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 15 sec @Thickness 3.17 mm |
15 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP310 Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500". |
|||
Arc Resistance | 15 sec @Thickness 3.17 mm |
15 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP310E Cotton Fabric Description: Manufactured with a domestic cotton fabric and phenolic resin. Similar to NP310 with improved moisture resistance and electrical properties. Mechanical properties equivalent to NP310. M.. |
|||
Arc Resistance | 15 sec @Thickness 3.17 mm |
15 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP320 Cotton Fabric Description: Fine weave (less than 4 ounce/square yard) cotton fabric commonly called linen, combined with phenolic resin to provide better machining than NP310. For smaller and more intricate shape.. |
|||
Arc Resistance | 15 sec @Thickness 3.17 mm |
15 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP320E Cotton Fabric Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500†|
|||
Arc Resistance | 15 sec @Thickness 3.17 mm |
15 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP320U Cotton Fabric Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500" |
|||
Arc Resistance | 15 sec @Thickness 3.17 mm |
15 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP310U Cotton Fabric Description: Utility grade canvas phenolic with properties similar to NP310E.Not certifiable to NEMA due to low crosswise flexural strength. Previously designated NP310C.Thickness Tested: 0.062", 0... |
|||
Arc Resistance | 15 sec | 15 sec | Practical Use (Water Absorption 1.9%); ASTM-D495 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 15 sec | 15 sec | Practical Use (Water Absorption 1.8%); ASTM-D495 |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |