Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 1.9 sec | 1.9 sec | |
Azoty Tarnow™ TARNOFORM 300 M POM Tribological modified grade with addition of molybdenum disulphide, which causes decreased coefficient of friction and wear, especially for applications requiring high load at low sliding speed.Info.. |
|||
Arc Resistance | 1.9 sec | 1.9 sec | ASTM D495 |
Azoty Tarnow™ TARNOFORM 300 POM Basic, fast cycling injection molding grade suitable for many applications.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Arc Resistance | 1.9 sec | 1.9 sec | |
Azoty Tarnow™ TARNOFORM 400 LS POM Injection molding grade based on Tarnoform 400 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Arc Resistance | 1.9 sec | 1.9 sec | |
Azoty Tarnow™ TARNOFORM 400 POM Easy flowing, fast cycling injection molding grade for manufacturing of thin-wall detailsInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Arc Resistance | 1.9 sec | 1.9 sec | |
Azoty Tarnow™ TARNOFORM 411 POM Easy flowing, internally strengthened grade for injection molding of thin walled parts of very high mechanical requirements.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Arc Resistance | 1.9 sec | 1.9 sec | |
Azoty Tarnow™ TARNOFORM 500 LS POM High flow injection molding grade based on Tarnoform 500 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Arc Resistance | 1.9 sec | 1.9 sec | |
Azoty Tarnow™ TARNOFORM 500 POM Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Arc Resistance | 1.9 sec | 1.9 sec | |
Azoty Tarnow™ TARNOFORM 700 POM Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Arc Resistance | 1.9 sec | 1.9 sec | ASTM D495 |
Azoty Tarnow™ TARNOFORM 200 LS POM Injection molding grade based on Tarnoform 200 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Arc Resistance | 1.9 sec | 1.9 sec | ASTM D495 |
Azoty Tarnow™ TARNOFORM 200 POM This material is a standard extrusion grade, also could be used for injection molding of low shape complexity details.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |