Polymer Property : Surface Resistivity per Square = 6.30e+10 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 6.30e+10 ohm

@Temperature 23.0 °C
6.30e+10 ohm

@Temperature 73.4 °F
100 V DC 66% RH; ASTM D257
DuPont Teijin Films Melinex® 514P Polyester Film
This high clarity film has one side hydrophilic pretreated to promote adhesion to many solvent coatings formulations, while the opposite side is pretreated to provide antistatic protection.Informati..