Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 10000 - 500000 ohm | 10000 - 500000 ohm | ASTM D257 |
PolyOne Stat-Tech™ ES-06CF-09GF/000 Polyethersulfone, Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |