Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 5.00e+10 ohm | 5.00e+10 ohm | 50% RH; ASTM D257 |
Lubrizol Stat-Rite® X-5076 Static Control High Impact Polystyrene Stat-Rite® X-5076 is a static dissipative, High Impact Polystyrene alloy. Stat-Rite® X-5076 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, p.. |
|||
Surface Resistivity per Square | 5.00e+10 ohm | 5.00e+10 ohm | ASTM D-257 |
Lubrizol Stat-Rite® X5166 Static Dissipative Polystyrene Compound Stat-Rite® X5166 is a static dissipative, High-Impact Polystyrene alloy. Stat-Rite® X5166 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, perm.. |
|||
Surface Resistivity per Square | 5.00e+10 ohm | 5.00e+10 ohm | Non-adhesive side; ASTM D257 |
3M 4718 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |