Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Lubrizol (former Noveon)
Trade Name Stat-Rite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Stat-Rite® X-5076 Static Control High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stat-Rite® X-5076 is a static dissipative, High Impact Polystyrene alloy. Stat-Rite® X-5076 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation properties when thermoformed into complex tray designs. Gardner Drop - Impact Strength is 1.0 in-lb/mil per ASTM D-5420-93.Features:Superior static decayClean: no sloughing, low offgassing, low ionicsConsistent ESD properties after thermoformingCarbon-free protectionApplications:Electronic component packagingTape & reelComponent handling traysProperties of all Stat-Rite® polymer products in the molten state are adversely affected by moisture. Although Stat-Rite® compounds are dry when packaged, trace amounts of moisture can be absorbed during storage and handling. Data provided by Noveon, Inc.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.5 MPa
2100 psi
ASTM D638-95
Elongation at Break 150 %
150 %
ASTM D638-95
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790-95A
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256-92
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Vicat Softening Point 94.0 °C
201 °F
ASTM D1525-95
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+11 ohm-cm
5.00e+11 ohm-cm
50% RH; ASTM D257
Surface Resistance 5.00e+9 ohm
5.00e+9 ohm
ESD S11.11; 50 % R.H.
Surface Resistivity per Square 5.00e+10 ohm
5.00e+10 ohm
50% RH; ASTM D257
Static Decay 0.30 sec
0.30 sec
FTMS-101C; 12% R.H., (+5000 V to 50 V)
1.5 sec
1.5 sec
Charged Plate Monitor (+1000 V to 100 V)
Descriptive Properties Value Comments
Color White