Surface Resistivity per Square 4.0 - 10 ohm
4.0 - 10 ohm
Parker Chomerics WIN-SHIELD™ ITO (Coated) EMI Shielded Window
Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast allycarbonate. A unique feature of Parker Chomerics w..
Surface Resistivity per Square 4.0 - 8.0 ohm
4.0 - 8.0 ohm
printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox
Gwent Electronic Materials C2110414D7 UV Silver Flexographic Ink
UV curable Silver conductor ink specifically designed for printing on to polymeric substrates using flexographic printing. Ink can be printed at speeds up to 13m/min, with good line definition and ..