Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1400 - 150000 ohm | 1400 - 150000 ohm | |
Panipol Oy T Inherently Conductive Polymer Doped polyaniline in tolueneSolution Processing, Coating formulations, Ink formulationsInformation provided by Panipol Oy Ltd |