Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.0e+10 - 1.0e+12 ohm | 1.0e+10 - 1.0e+12 ohm | IEC 60093 |
Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data) Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors fo.. |
|||
Surface Resistivity per Square | 1.0e+10 - 1.0e+12 ohm | 1.0e+10 - 1.0e+12 ohm | IEC 60093 |
Quadrant EPP Semitron® ESd 500HR PTFE, static dissipative, extruded (ISO Data) Reinforced with a proprietary synthetic mica, Semitron ESd 500HR offers an excellent combination of low frictional properties, good dimensional stability and electrostatic dissipation. Whenever virg.. |