Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data)

Category Polymer , Thermoplastic , Polyamide-imide (PAI)
Manufacturer Quadrant Engineering Plastics Products
Trade Name Semitron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors for test equipment and other device handling components in the semiconductor industry
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 2.6 %
2.6 %
50% RH
Water Absorption at Saturation 4.6 %
4.6 %
Mechanical Properties Metric English Comments
Hardness, Rockwell E 73
73
Hardness, Shore D 90
90
Ball Indentation Hardness 250 MPa
36300 psi
ISO 2039-1
Tensile Strength 83.0 MPa
12000 psi
at Break (NYP); ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
ISO 527-1/-2
Tensile Modulus 5.50 GPa
798 ksi
ISO 527-1/-2
Flexural Strength 105 MPa
15200 psi
Compressive Strength 42.0 MPa

@Strain 1 %
6090 psi

@Strain 1 %
ISO 604
80.0 MPa

@Strain 2 %
11600 psi

@Strain 2 %
ISO 604
145 MPa

@Strain 5 %
21000 psi

@Strain 5 %
ISO 604
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179-1/1eA
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C

@Temperature 23.0 - 100 °C
19.4 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.340 W/m-K
2.36 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 250 °C
482 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 280 °C
536 °F
ISO 75-1/-2
Glass Transition Temp, Tg 280 °C
536 °F
DSC, 20°C/min.; ISO 11357-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index 48 %
48 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.0e+10 - 1.0e+12 ohm-cm
1.0e+10 - 1.0e+12 ohm-cm
IEC 60093
Surface Resistivity per Square 1.0e+10 - 1.0e+12 ohm
1.0e+10 - 1.0e+12 ohm
IEC 60093
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative Yes
Yes
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable