Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 0.016 ohm | 0.016 ohm | fired; 8 microns thick |
Gwent Electronic Materials C2000808D2 Silver Backlight Ink Silver Ink C2000808D2 is a high resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has dark color when printed and fired on floa.. |