Polymer Property : Surface Resistivity per Square = 0.016 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.016 ohm
0.016 ohm
fired; 8 microns thick
Gwent Electronic Materials C2000808D2 Silver Backlight Ink
Silver Ink C2000808D2 is a high resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has dark color when printed and fired on floa..