Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 60 V | 60 V | IEC 60112 |
GEHR Plastics PA 12 TR Transparent Nylon 12 Used for optical components that benefit from the transparency and the high dynamic strengthProperties:TransparencyExtremely high dynamic strengthHigh chemical resistanceHigh stress-cracking resista.. |
|||
Comparative Tracking Index | 60 V | 60 V | Solution A; IEC 60112 |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Comparative Tracking Index | 60 V | 60 V | Solution A; IEC 60112 |
Solvay TECHNYL® C 50 H2 PA6, Conditioned Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Comparative Tracking Index | 60 V | 60 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® LBV-50H FWA nat PA12-GF50 Product Description: Grilamid LBV-50H FWA natural is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |