Polymer Property : Comparative Tracking Index = 425 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Comparative Tracking Index 425 V
425 V
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Comparative Tracking Index 425 V
425 V
Plastcom SLOVASTER® B1 HML GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Comparative Tracking Index 425 V
425 V
IEC 60112
Celanese Celanex® 2300 GV1/30 PBT, 30% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: PBTGeneral purpose, 30% glass fiber reinforced PBTInformation provided by Celanese
Comparative Tracking Index 425 V
425 V
IEC 60112
Celanese Celanex® 3309HR PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HR is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass reinforced, hyd..
Comparative Tracking Index 425 V
425 V
IEC 60112
Celanese Vandar® 4612R PBT, 7% Glass Reinforced  (Unverified Data**)
Vandar 4612R is a high impact polyester alloy containing 7% glass. It possesses excellent impact properties as well as toughness and moldability. Dimensional stability, chemical resistance, and low ..
Comparative Tracking Index 425 V
425 V
IEC 60112
Celanese Vandar® 4662Z PBT, 30% Glass Reinforced  (Unverified Data**)
Vandar 4662Zis a high impact polyester alloy which contains 30% glass fiber loading. It is characterized by toughness, dimensional stability, and high modulus. Good weatherability and moldability ar..
Comparative Tracking Index 425 V
425 V
Solution A; IEC 60112
Polimeri Europa Edistir N 2380 Polystyrene
High molecular weight general purpose polystyrene combining high heat resistance and good mechanical strength. Suitable for direct gassing extrusion, for biaxially oriented films and sheets, for gla..
Comparative Tracking Index 425 V
425 V
d.a.m.; Solution A; IEC 60112
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Comparative Tracking Index 425 V
425 V
IEC 60112
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow)
Comparative Tracking Index 425 V
425 V
IEC 60112
Lanxess Durethan® BKV 35 HTS 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, very good heat-ageing resistance
Comparative Tracking Index 425 V
425 V
IEC 60112
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures
Comparative Tracking Index 425 V
425 V
Solution A; IEC 60112
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, Conditioned
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail..
Comparative Tracking Index 425 V
425 V
Solution B; IEC 60112
Solvay TECHNYL® B 218 Black 21 N PA66/6, DRY
Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® B 218 offers all of the primary proper..
Comparative Tracking Index 425 V
425 V
Solution A; IEC 60112
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, Conditioned
Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15..
Comparative Tracking Index 425 V
425 V
IEC 60112
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA
Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, ..
Comparative Tracking Index 425 V
425 V
IEC 60112
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific)
Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, ..
Comparative Tracking Index 425 V
425 V
Solution A; IEC 60112
Solvay TECHNYL® 2412GHF6 PA66, 33% glass fiber, Conditioned
Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF6 is used in all sectors of indu..
Comparative Tracking Index 425 V
425 V
ASTM D3638
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Comparative Tracking Index 425 V
425 V
dry; IEC 60112
DSM Stanyl® SC50 PA46-GF30 FR
30% Glass Reinforced, Flame Retardant, Halogen free and free of red phosphorous
Comparative Tracking Index 425 V
425 V
IEC 60112
Eurostar Staramide BT6 PA6, 30% Mineral Filled, Injection Molded
Staramide BT6 is a 30% Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Comparative Tracking Index 425 V
425 V
IEC 60112
DSM Akulon® K224-HG3 (Dry) 15% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Comparative Tracking Index 425 V
425 V
conditioned; IEC 60112
EMS-Grivory Grivory® EB 50 H DZ PA6
Product description: Grilon EB 50 H DZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon EB 50 H DZ has the following important properties:..
Comparative Tracking Index 425 V
425 V
IEC 60112
Eurostar Starflam AFR662B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR662B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Comparative Tracking Index 425 V
425 V
IEC 60112
Celanese CELANEX 2300 GV1/30 PBT, 30% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: PBTInformation provided by Celanese
Comparative Tracking Index 425 V
425 V
IEC 60112
Celanese CELANEX 3300 PBT, 30% Glass Reinforced
Ceanex 3300 is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outstandi..
Comparative Tracking Index 425 V
425 V
IEC 60112
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Comparative Tracking Index 425 V
425 V
IEC 60112
Celanese CELANEX 3309HR PBT, 30% Glass Reinforced
Celanex 3309HR is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.Information provided by C..
Comparative Tracking Index 425 V
425 V
IEC 60112
Celanese CELANEX XFR 6842 GF15 PBT, 30% Glass Reinforced
Celanex XFR 6842 GF15 is a halogen and antimony free flame retardant (V-0 @ 0.4 mm) 15% glass reinforced PBT grade with good processability and no corrosive emissions during processing. It is suita..
Comparative Tracking Index 425 V
425 V
Test solution A; IEC 60112
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry)
Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele..
Comparative Tracking Index 425 V
425 V
IEC 60112
Celanese Celanex® 3300D PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..