Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 295 V | 295 V | IEC 112 |
LATI LATAMID 12 H FE85 Nylon 12 Base Magnetizable Compound
(discontinued **) Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us.. |