Polymer Property : Surface Resistance = 5.00e+14 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance >= 5.00e+14 ohm

@Temperature 23.0 °C
>= 5.00e+14 ohm

@Temperature 73.4 °F
25% r.h.; DIN 53482 or VDE 0303/part 3
Mitsubishi Hostaphan® RN, 36 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin..
Surface Resistance >= 5.00e+14 ohm

@Temperature 23.0 °C
>= 5.00e+14 ohm

@Temperature 73.4 °F
50% r.h.; DIN 53482 or VDE 0303/part 3
Mitsubishi Hostaphan® RN, 36 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin..
Surface Resistance >= 5.00e+14 ohm

@Temperature 23.0 °C
>= 5.00e+14 ohm

@Temperature 73.4 °F
25% r.h.; DIN 53482 or VDE 0303/part 3 or ASTM D257
Mitsubishi Hostaphan® WN, 190 micron Nominal Thickness Translucent White Polyethylene Terephthalate Film
Hostaphan® WN is a white film made of polyethylene terephthalate (PET) and is well suited for electrical insulating of machines and appliances. The high dielectric strength and large volume resis..
Surface Resistance 5.00e+14 ohm

@Temperature 23.0 °C
5.00e+14 ohm

@Temperature 73.4 °F
50%RH; ASTM D257
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon
Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona..