Electrical Properties Metric English Comments
Surface Resistance 1.00e+11 ohm

@Temperature 23.0 °C
1.00e+11 ohm

@Temperature 73.4 °F
50%RH; ASTM D257
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Surface Resistance 1.00e+11 ohm

@Temperature 23.0 °C
1.00e+11 ohm

@Temperature 73.4 °F
50%RH; IEC 60093
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers