Polymer Property : Electrical Resistivity = 1.50e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.50e+13 ohm-cm

@Temperature 65.6 °C
1.50e+13 ohm-cm

@Temperature 150 °F
Abatron AboCast 8-15/Abocure 8-15 Epoxy  (discontinued **)
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/11.80 ratio (pbw); Gel time, 100 g (3.5 oz.): 70 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°..