Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.40e+11 ohm-cm @Temperature 65.6 °C |
1.40e+11 ohm-cm @Temperature 150 °F |
|
Abatron AboCast 8-18/Abocure 8-18 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/32.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 120 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c.. |