Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | <= 1.00e+9 ohm-cm @Temperature 93.3 °C |
<= 1.00e+9 ohm-cm @Temperature 200 °F |
|
Abatron AboCast 8-8/Abocure 8-8 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 135 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)... |
|||
Electrical Resistivity | <= 1.00e+9 ohm-cm @Temperature 93.3 °C |
<= 1.00e+9 ohm-cm @Temperature 200 °F |
|
Abatron AboCast 8-10/Abocure 8-10 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/35 ratio (pbw); Gel time, 1 lb. (2.2 kg): 45 minutes; cures in 6 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F).Ap.. |
|||
Electrical Resistivity | 1.00e+9 ohm-cm @Temperature 93.3 °C |
1.00e+9 ohm-cm @Temperature 200 °F |
|
Abatron AboCast 8-11/Abocure 8-11 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/35 ratio (pbw); Gel time, 100 g (3.5 oz.): 93 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adhe.. |