Material Notes:
2-part solvent-free dielectric epoxy casting compound.Processing: 100/35 ratio (pbw); Gel time, 100 g (3.5 oz.): 93 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adhesive, and coating.
Physical Properties Metric English Comments
Water Absorption 0.20 %
0.20 %
in 24 hours.
Viscosity Measurement 700
700
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
Tensile Strength, Ultimate 57.23 MPa
8301 psi
Elongation at Break 4.0 %
4.0 %
Flexural Strength 92.39 MPa
13400 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 84.0 °C
183 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+9 ohm-cm

@Temperature 93.3 °C
1.00e+9 ohm-cm

@Temperature 200 °F
1.00e+11 ohm-cm

@Temperature 65.6 °C
1.00e+11 ohm-cm

@Temperature 150 °F
2.00e+15 ohm-cm

@Temperature 25.0 °C
2.00e+15 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 3.68

@Frequency 1e+6 Hz
3.68

@Frequency 1e+6 Hz
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Curing time: 3 weeks