Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000080280 ohm-cm @Temperature 22.0 °C |
0.000080280 ohm-cm @Temperature 71.6 °F |
0.100-in Cold-Rolled Plate; ASTM B-63 |
Special Metals INCOLOY® alloy 832 Stainless Steel INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula.. |