Polymer Property : Electrical Resistivity = 0.000080280 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.000080280 ohm-cm

@Temperature 22.0 °C
0.000080280 ohm-cm

@Temperature 71.6 °F
0.100-in Cold-Rolled Plate; ASTM B-63
Special Metals INCOLOY® alloy 832 Stainless Steel
INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula..