Polymer Property : Surface Resistance = 7.00e+14 ohm
Polymer Property :
Surface Resistance =
7.00e+14 ohm
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Surface Resistance
7.00e+14
ohm
7.00e+14
ohm
BASF Ultramid® B36 LN 0.04 mm Cast Film Cold Chillroll
Product comes in 2-2.5 mm round pellets.Information provided by BASF