BASF Ultramid® B36 LN 0.04 mm Cast Film Cold Chillroll

Category Polymer , Film , Thermoplastic , Nylon
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B36 LN 0.04 mm Cast Film Cold Chillroll.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product comes in 2-2.5 mm round pellets.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.640 - 0.740 g/cc
0.0231 - 0.0267 lb/in³
Density 1.12 - 1.15 g/cc
0.0405 - 0.0415 lb/in³
Water Absorption 9.5 %
9.5 %
saturation in water 23°C
Moisture Absorption at Equilibrium 2.6 %
2.6 %
23°C/50% RH
Water Vapor Transmission 28.0 g/m²/day
1.80 g/100 in²/day
85% RH
Oxygen Transmission Rate 14.0 cc/m²/day
0.902 cc/100 in²/day
50% RH
Viscosity Measurement 3.49 - 3.71
3.49 - 3.71
(RV) 1% [m/v] in 96% [m/m] sulfuric acid; ISO 307
210 - 226
210 - 226
(RV) 0.5% [m/v] in 96% [m/m] sulfuric acid; ISO 307
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.0 MPa
10900 psi
TD
75.0 MPa
10900 psi
MD
Elongation at Break 380 %
380 %
MD
400 %
400 %
TD
Tensile Modulus 0.650 GPa
94.3 ksi
MD
0.700 GPa
102 ksi
TD
Thermal Properties Metric English Comments
Specific Heat Capacity 1.50 J/g-°C
0.359 BTU/lb-°F
Melting Point 220 °C
428 °F
Decomposition Temperature >= 300 °C
>= 572 °F
Electrical Properties Metric English Comments
Surface Resistance 7.00e+14 ohm
7.00e+14 ohm
Processing Properties Metric English Comments
Moisture Content 0.060 %
0.060 %
ISO 15512
Descriptive Properties Value Comments
Commercial Status Europe
Extractables <0.6 %
ISO 6427
Ignition Temperature >400°C
ASTM D1929
Nucleating Agent 250 - 550 mg/kg
BASF