Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 5.00e+8 - 5.00e+12 ohm | 5.00e+8 - 5.00e+12 ohm | ASTM D257 |
PolyOne Stat-Tech™ PC-08CF/000 FR V0 Polycarbonate (PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Surface Resistance | 1.00e+11 - 5.00e+12 ohm | 1.00e+11 - 5.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTU PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency, UV cut, and superior cleanliness for advanced semiconductor packaging applications |