Surface Resistance 4.10e+13 ohm
4.10e+13 ohm
d.a.m.; IEC 60093
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.