Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.90e+14 - 3.90e+14 ohm @Temperature 149 - 149 °C |
3.90e+14 - 3.90e+14 ohm @Temperature 300 - 300 °F |
Average value: 3.90e+14 ohm Grade Count:1 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |