Electrical Properties Metric English Comments
Surface Resistance 3.90e+14 - 3.90e+14 ohm

@Temperature 149 - 149 °C
3.90e+14 - 3.90e+14 ohm

@Temperature 300 - 300 °F
Average value: 3.90e+14 ohm Grade Count:1
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..