Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.09e+13 - 3.87e+13 ohm | 3.09e+13 - 3.87e+13 ohm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP DZ004 PC (Asia Pacific) LNP* Thermocomp* DZ004 is a compound based on Polycarbonate resin containing Glass Fiber. Also known as Thermocomp DF-1004 M |