Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.50e+6 - 6.10e+17 ohm | 3.50e+6 - 6.10e+17 ohm | Average value: 4.71e+16 ohm Grade Count:19 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Surface Resistance | 3.50e+6 ohm | 3.50e+6 ohm | Cured property; ETS 860B |
Aptek 2214-A/B Low modulus urethane ESD coating/adhesive Space Grade, Low modulus urethane ESD coating/adhesiveAPTEK is a carbon-filled, thixotropic, two component, electrically conductive, flexible urethane coating/adhesive designed to dissipate an elect.. |