Electrical Properties Metric English Comments
Surface Resistance 110000 - 250000 ohm
110000 - 250000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific)
Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications.