Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 25000 ohm | >= 25000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP KONDUIT OX10324 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound, with through-plane and in-plane thermal conductivity of 3.5 W/(m*K) and 15 W/(m*K) respectively, conforming to ASTM E 1461 test standard. |
|||
Surface Resistance | 25000 ohm | 25000 ohm | ASTM D257 |
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat.. |