SABIC Innovative Plastics LNP KONDUIT OX10324 PPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Konduit
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP KONDUIT OX10324 PPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermally conductive mineral filled PPS FR compound, with through-plane and in-plane thermal conductivity of 3.5 W/(m*K) and 15 W/(m*K) respectively, conforming to ASTM E 1461 test standard.
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
Water Absorption 0.010 %

@Time 86400 sec
0.010 %

@Time 24.0 hour
SABIC Method
Linear Mold Shrinkage, Flow 0.0016 cm/cm

@Time 86400 sec
0.0016 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.0 MPa
7110 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 0.60 %
0.60 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 13.5 GPa
1960 ksi
5 mm/min; ASTM D638
Flexural Strength 75.0 MPa
10900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 15.6 GPa
2260 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.240 J/cm
0.450 ft-lb/in
ASTM D256
Izod Impact, Unnotched 0.700 J/cm
1.31 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 13.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
7.33 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 258 °C

@Thickness 6.40 mm
496 °F

@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 130 °C
266 °F
UL 746B
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
Flammability, UL94 V-0

@Thickness 1.20 mm
V-0

@Thickness 0.0472 in
UL 94
Glow Wire Test 850 °C
1560 °F
IEC 60695-2-13
Electrical Properties Metric English Comments
Surface Resistance >= 25000 ohm
>= 25000 ohm
ASTM D257
Users viewing this material also viewed the following: