Electrical Properties Metric English Comments
Surface Resistance 1.00e+12 - 2.00e+15 ohm
1.00e+12 - 2.00e+15 ohm
Average value: 6.40e+14 ohm Grade Count:8
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..