Electrical Properties Metric English Comments
Surface Resistance 19000 ohm
19000 ohm
IEC 93
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor..