Polymer Property : Surface Resistance = 150 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 150 ohm
150 ohm
ASTM D257
Saint-Gobain Meldin® 1003 Thermoplastic Bearing Material
Meldin 1003 components offer the highest level of strength and rigidity for this product family. They maintain high chemical, tensile, and flexural properties even at elevated temperatures.MeldinÂ..