Material Notes:
Meldin 1003 components offer the highest level of strength and rigidity for this product family. They maintain high chemical, tensile, and flexural properties even at elevated temperatures.Meldin® 1000 series components are used in appliance applications due to their superior wear life and ability to operate without the need for any oils or lubricants. For scroll tip seal applications, Meldin® 1000 series materials provide some parts with superior wear resistance properties, and superior deformation properties over those of standard PTFE scroll tip seals. In vehicle systems such as transmission bearings or thrust washers, as well as fuel pump bearings, Meldin® 1000 series materials provide performance superior to metallic components. The Meldin 1000 series materials' wear resistance, coupled with their excellent chemical resistance, make them ideal materials for vehicle system components.
Physical Properties Metric English Comments
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength 46.0 MPa

@Temperature 204 °C
6670 psi

@Temperature 399 °F
ASTM D 638
69.0 MPa

@Temperature 149 °C
10000 psi

@Temperature 300 °F
ASTM D 638
175 MPa

@Temperature 25.0 °C
25400 psi

@Temperature 77.0 °F
ASTM D 638
Elongation at Break 2.0 %

@Temperature 23.0 °C
2.0 %

@Temperature 73.4 °F
ASTM D 638
2.5 %

@Temperature 149 °C
2.5 %

@Temperature 300 °F
ASTM D 638
2.8 %

@Temperature 204 °C
2.8 %

@Temperature 399 °F
ASTM D 638
Flexural Strength 193 MPa
28000 psi
ASTM D 790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D 790
Compressive Strength 23.4 MPa

@Temperature 204 °C
3390 psi

@Temperature 399 °F
ASTM D 695
38.0 MPa

@Temperature 149 °C
5510 psi

@Temperature 300 °F
ASTM D 695
155 MPa

@Temperature 23.0 °C
22500 psi

@Temperature 73.4 °F
ASTM D 695
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 1.40 µm/m-°C
0.778 µin/in-°F
ASTM E831-93
Thermal Conductivity 0.750 W/m-K
5.20 BTU-in/hr-ft²-°F
ASTM F433
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 150 ohm
150 ohm
ASTM D257