Electrical Properties Metric English Comments
Surface Resistance 9.0 - 11 ohm
9.0 - 11 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6
LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat.
Surface Resistance 9.0 - 11 ohm
9.0 - 11 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6
LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat.