Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 9.0 - 11 ohm | 9.0 - 11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6 LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat. |
|||
Surface Resistance | 9.0 - 11 ohm | 9.0 - 11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6 LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat. |