Polymer Property : Surface Resistance = 1.90e+17 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 - 1.90e+17 ohm
1.00e+16 - 1.90e+17 ohm
Average value: 1.54e+17 ohm Grade Count:5
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Surface Resistance 1000 - 1.90e+17 ohm
1000 - 1.90e+17 ohm
Average value: 1.06e+16 ohm Grade Count:36
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..