Polymer Property : Surface Resistance = 1.80e+15 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 3000 - 1.80e+15 ohm
3000 - 1.80e+15 ohm
Average value: 1.25e+14 ohm Grade Count:19
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..