Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Surface Resistance = 1.51 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 1.51 ohm
1.51 ohm
IEC 93
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Copyright © lookpolymers.com All Rights Reserved