Polymer Property : Surface Resistance = 1.19e+16 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance >= 1.19e+16 ohm
>= 1.19e+16 ohm
Abatron AboCast 50-11/AboCure 50-12 Epoxy
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/13.5 ratio. Pot life: 500 g, 36 min. at 25°C (77°F). Exothermic Peak 265°C (510°F). Hardens in 2-24 hou..